Cracks / Honeycombs

  • Clean any dirt or loose material from the area
  • Wet the cleaned area before applying the repair material
  • Fill small voids and cracks using a mechanical injection pressure pump with a suitable material such as non-shrinkage epoxy grout.
  • If the honeycomb covers a large area, you may need to create a patch hole to ensure proper bonding.
  • Place formworks if necessary, and pour the grout.
  • If formwork is not used, apply suitable repair material such as non-shrinkage, high-strength grout.
  • The filling process should be in a 15 mm thickness layer if the depth of honeycombing is greater than 5 cm. It is recommended to wait for a while (30min) before applying the next layer.
  • Repair material strength should match the virgin concrete of the structural element.
  • Provide texture and color required to match the surrounding concrete and maintain aesthetics.
  • If present, remove formworks after 12 hours of repair based on the type of material used and ambient conditions. Cure repair material to gain adequate strength.